CuNi10Fe1Mn1-B ( CB380H )



| Gradd : | CuNi10Fe1Mn1-B |
| Rhif: | CB380H |
| Dosbarthiad: | Aloi copr-nicel |
| Safon: | EN 1982: 2008 Copr ac aloion copr. Ingotau a castiau |
| Graddau cyfwerth: | Dim gwybodaeth |
Cyfansoddiad cemegol % gradd CuNi10Fe1Mn1-B ( CB380H )
| Ychwanegir ôl-ddodiad -B at y dynodiad i adnabod defnydd ar ffurf ingotau |
| Fe | C | Os | Mn | Ni | Ds | Al | Cu | Pb | Zn |
| 1.2 - 1.8 | uchafswm 0.1 | uchafswm 0.1 | 1.2 - 1.5 | 9.2 - 11 | uchafswm 1 | uchafswm 0.01 | min 84.5 | uchafswm 0.03 | uchafswm 0.5 |
Priodweddau mecanyddol gradd CuNi10Fe1Mn1-B ( CB380H )
| Rm- Cryfder tynnol (MPa) (GS) | 280 |
| Rm- Cryfder tynnol (MPa) (GZ) neu (GC) | 280 |
| Rp0.20.2% cryfder prawf (MPa) (GS) | 120 |
| Rp0.20.2% cryfder prawf (MPa) (GZ) neu (GC) | 100 |
| A— Min. hiriad wrth dorri asgwrn (%) (GS) | 20 |
| A— Min. hiriad wrth dorri asgwrn (%) (GZ) neu (GC) | 25 |
| Caledwch Brinell (HBW): (GS) neu (GZ) neu (GC) | 70 |
Proses castio
| GS | Castio tywod |
| GM | Castio llwydni parhaol |
| GZ | Castio allgyrchol |
| GC | Castio parhaus |
| Meddyg Teulu | Castio marw pwysau |
Amodau materol
| R | Cyflwr materol a ddynodwyd gan y gwerth lleiaf o gryfder tynnol gofyniad ar gyfer y cynnyrch gyda chryfder tynnol gorfodol a gofynion elongation |
| H | Cyflwr materol a ddynodwyd gan y gwerth lleiaf o ofyniad caledwch ar gyfer y cynnyrch gyda gofynion caledwch gorfodol |
Priodweddau mecanyddol
| REh | Cryfder cnwd lleiaf / Mindestwert der oberen Streckgrenze / Limite d elastigit minimale |
| Rm | Cryfder tynnol / Zugfestigkeit / Resistance a la traction |
| A | Lleiafswm elongation / Mindestwert der Bruchdehnung / Allongement minimal |
| J | Prawf effaith rhicyn / Kerbschlagbiegeversuch / Essai de flexion par choc |
|
CuNi10Fe1Mn1-B ( CB380H ) Aloi copr-nicel |